Optical fiber structure characteristics |
Unit |
Requirement |
|
Cladding diameter |
μm |
125±0.7 |
|
Cladding non-circularity |
% |
≤0.8 |
|
Core/Cladding concentricity error |
μm |
≤0.5 |
|
Primary coating diameter |
μm |
155±5 |
|
Second coating diameter |
μm |
200±10 |
|
Excentric core |
% |
≥70 |
|
Cladding / coating concentricity error |
μm |
≤10.0 |
|
MFD(1310nm) |
μm |
8.6±0.4 |
|
|
Cut-off wavelengths λc |
μm |
1.18~1.33 |
|
|
Attenuation coefficient |
1310nm |
dB/km |
≤0.35 |
|
1383nm |
dB/km |
≤0.33 |
|
|
1550nm |
dB/km |
≤0.21 |
|
|
1625nm |
dB/km |
≤0.24 |
|
|
Macro bending loss |
Bending radius |
mm |
15 |
|
Circle number |
Mm |
10 |
|
|
1550nm,max. |
dB |
0.03 |
|
|
1625nm,max. |
dB |
0.1 |
|
|
Attenuation wavelength characteristics |
1285nm~1330nm |
dB/km |
≤0.03 |
|
1525nm~1575nm |
dB/km |
≤0.02 |
|
|
Attenuation point discontinuity 1310nm 1383nm 1550nm 1625nm |
dB |
≤0.015 ≤0.03 ≤0.03 ≤0.03 |
|
|
Dispersion coefficient, 1288nm~1339nm |
ps/nm.k |
|D|≤5.3 |
|
|
Dispersion coefficient, 1271nm~1360nm |
ps/nm.k |
|D|≤3.4 |
|
|
Dispersion,1550nm |
ps/nm.k |
≤17.5 |
|
|
Zero dispersion wavelength |
nm |
1300~1322 |
|
|
Zero dispersion slope |
ps/nm2.k |
≤0.091 |
|
|
PMD(Fiber link value-uncabled) |
ps/km1/2 |
≤0.2 |
|
|
Optical fiber mechanical properties: |
Unit |
Requirement |
|
Proof test |
GPa |
≥0.79 |
|
Bending radius |
m |
≥5.0 |
|
Torsion |
Turns |
≤0.5 |
|
Dynamic fatigue parameters |
nd |
≥20 |
|
Coating peel force |
N |
1.3≤FPeak ≤8.9
1.0≤Faverage≤5.0
|
|
Optical fiber environment performance |
||
|
Temperature cycling test : from -60℃ to 85℃ |
dB/km |
≤0.03 |
|
Watersoak test: at 23℃, for 30 days |
dB/km |
≤0.03 |
|
Damp heat test: at 85℃ and 85% RH, for 30 days |
dB/km |
≤0.03 |
|
Dry heat aging test: at 85℃ |
dB/km |
≤0.03 |